I have trouble fixing the terrible seams I’m getting. I’ve followed Elli’s print tuning guide and calibrated extruder, tuned PA (it’s now 0.035) and extrusion multiplier.

I’ve tried adjusting both retraction length and speed, but it doesn’t seem to have much impact. I’m not using “wipe on retract” or “retract on layer change”, I only retract if travel distance is longer than 3mm. Retract is 0.3mm @35mm/s.

I’ve tried reducing PA smooth time too, but this also doesn’t seem to have a noticable impact.

I’ve tried reducing seam gap from the default 10% in Orca all the way down to 0%, but the bad seams persist.

I’ve tried with “wipe on loops” both disabled and enabled with no difference.

I’ve tried with both arachne and classic wall generator, no difference.

I’ve tried different wall orders, inner/outer, inner/outer/inner and outer/inner, all with the same bad seams.

Filament in the picture is matte PLA, it is without doubt dry and generally prints well aside from the seams. It’s stored vacuum sealed with silica, and I use a filament dryer to dry if I suspect wet filament.

I’m running out of ideas for where to tweak to get a decent result.

    • DreadPotato@sopuli.xyzOP
      link
      fedilink
      English
      arrow-up
      2
      ·
      10 months ago

      Tried without PA but there was no difference, going to try different filament next.

      As I mentioned somewhere else in this post, it seems to relate to the infill. I’m using gyroid, and the seam lines up with the anchor point for the infill.

      • rambos@lemm.ee
        link
        fedilink
        English
        arrow-up
        2
        ·
        10 months ago

        You can also try without infill 😉

        Im throwing many things to try, but not in any particular order

    • rambos@lemm.ee
      link
      fedilink
      English
      arrow-up
      2
      ·
      10 months ago

      Also try normal brass nozzle and check if your new hotend is not loose